MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayflex® 257 Polyether-based Polyurethane System
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Characterization: Bayflex 257 is a fully compounded polyether-based polyurethane system consisting of two liquid components which can be water-blown.

Properties / Applications: Bayflex 257 is a fully compounded polyether-based polyurethane system consisting of two liquid components which can be water-blown. Component A is a modified diphenylmethane diisocyanate (MDI) prepolymer, and Component B is a polyether polyol system. The Bayflex 257 system is used in the outsole system of dual-density polyether shoe soles. Finished outsoles can be molded translucent to opaque. The combination of durability, styling latitude and ease of processing makes the Bayflex 257 system a prime soling material for dual-density soles for casual, walking and light-duty shoes. As with any product, use of the Bayflex 257 system in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccMolded
 1.05 g/cc1.05 g/ccPolyol (Component B)
 1.21 g/cc1.21 g/ccIsocyanate (Component A)
Viscosity 550 - 800 cP550 - 800 cPIsocyanate (Component A)
 1100 cP1100 cPPolyol (Component B)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 55 - 6055 - 60ASTM D2240
Tensile Strength at Break 8.27 - 10.3 MPa1200 - 1490 psiASTM D412
Elongation at Break 500 - 600 %500 - 600 %ASTM D412
Tear Strength 35.1 - 43.8 kN/m200 - 250 pliDie C; ASTM D1004
Taber Abrasion, mg/1000 Cycles 50
@Load 1.00 kg
50
@Load 2.20 lb
H-18; ASTM D4060
 
Thermal PropertiesMetricEnglishComments
Flash Point 135 °C275 °FPolyol (Component B)
 213 °C415 °FIsocyanate (Component A)
 
Processing PropertiesMetricEnglishComments
Mold Temperature 49.0 °C120 °F
 
Descriptive Properties
AppearanceLight yellow liquidPolyol (Component B)
 Light yellow to yellow liquidIsocyanate (Component A)
Content22.6-23.1%NCO, Isocyanate (Component A)
Hydroxyl number[mg KOH/g], Polyol (Component B)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Texin® 5286 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Texin® 5290 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Bayflex® 970 Polyether-based Polyurethane System, Density 34 pcf
Covestro Texin® 5250 Thermoplastic Polyurethane, Polyether-based, Medical
Covestro Texin® DP7-3006 Thermoplastic Polyurethane, Polyether-based, Aliphatic

PCOVEST0124 / 201907

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.