MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Zytel® 73G45L NC010 PA6-GF45
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: 45% Glass Reinforced Polyamide 6

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.51 g/ccDAM; ISO 1183
Water Absorption 4.9 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Moisture Absorption 1.70 %
@Thickness 2.00 mm
DAM; Sim. to ISO 62
Viscosity Number 148 cm³/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0010 cm/cmDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cmDAM; ISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 250 MPaH 961/30; DAM; ISO 2039-1
Tensile Strength at Break 160 MPa50% RH; ISO 527-1/-2
 230 MPaDAM; ISO 527-1/-2
Elongation at Break 3.0 %DAM; ISO 527-1/-2
 5.0 %50% RH; ISO 527-1/-2
Tensile Modulus 9700 MPa50% RH; ISO 527-1/-2
 14500 MPaDAM; ISO 527-1/-2
Flexural Strength 310 MPaDAM; ISO 178
Flexural Modulus 13000 MPaDAM; ISO 178
Compressive Strength 170 MPa50% RH; ISO 604
Poissons Ratio 0.33DAM
 0.3450% RH
Shear Strength 60.0 MPa50% RH; ASTM D 732
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 18.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 24.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 101 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 111 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
 115 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 115 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
Charpy Impact, Notched 19.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 23.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 25.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Tensile Creep Modulus, 1 hour 9400 MPa1h; 50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 7300 MPa1000h; 50% RH; ISO 899-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 16.0 µm/m-°CDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°CDAM; ISO 11359-1/-2
Melting Point 221 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 221 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 213 °CDAM; ISO 75-1/-2
Vicat Softening Point 215 °C50°C/h, 50N; DAM; ISO 306
Glass Transition Temp, Tg 15.0 °C10°C/min; 50% RH; ISO 11357-1/-2
 55.0 °C10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 1.50 mm
DAM; IEC 60695-11-10
Flame Spread 44.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 270 °COptimum, Injection
 260 - 280 °CRange, Injection
Mold Temperature 70.0 - 120 °CInjection
 100 °COptimum, Injection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 50.0 - 100 MPaRange, Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA6,GF45,M1GNR,S14-140
Max. screw tangential speed (m/s)0.2Injection
Part Marking Code>PA6-GF45<ISO 11469
PolymerPA6-GF45
Processing Hold Pressure Time (s/mm)3Injection
Resin IdentificationPA6-GF45ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 73G45 BK263 PA6-GF45
Envalior Novamid® 1013G45 1 NA PA6-GF45
Celanese Minlon® 73M40 NC010 PA6-MD40
Envalior Novamid® 1013GH45 1 NA/BK701 PA6-GF45
Celanese Zytel® 80G14A NC010A PA66-IGF14

PDSX5362 / 198002

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.