MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company EMI 161 Z Polypropylene (PP); Stainless Steel Fiber - Electrically Conductive - EMI/RFI/ESD Protection - FDA Compliant Ingredients
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Stainless Fiber, EMI

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.990 g/ccASTM D 792
Linear Mold Shrinkage 0.010 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 3000 psiASTM D 638
Elongation at Break >= 10 %ASTM D 638
Tensile Modulus 140 ksiASTM D 638
Flexural Strength 4500 psiASTM D 790
Flexural Modulus 180 ksiASTM D 790
Izod Impact, Notched 4.50 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 10 ohm-cmASTM D 257
Surface Resistance <= 10000 ohmESD STM11.11
Surface Resistivity per Square <= 1e+05ASTM D 257; ESD STM11.11
Static Decay <= 2.0 secFTMS101C; 4046.1
Shielding Effectiveness 46 dB
@Thickness 2.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 46 dB
@Thickness 2.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 46 dB
@Thickness 2.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 47 dB
@Thickness 2.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 48 dB
@Thickness 2.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 53 dB
@Thickness 2.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 58 dB
@Thickness 3.00 mm,
Frequency 3.00e+8 Hz
ASTM D 4935
 61 dB
@Thickness 3.00 mm,
Frequency 5.00e+8 Hz
ASTM D 4935
 63 dB
@Thickness 3.00 mm,
Frequency 7.00e+8 Hz
ASTM D 4935
 64 dB
@Thickness 3.00 mm,
Frequency 1e+9 Hz
ASTM D 4935
 68 dB
@Thickness 3.00 mm,
Frequency 1.30e+9 Hz
ASTM D 4935
 70 dB
@Thickness 3.00 mm,
Frequency 1.50e+9 Hz
ASTM D 4935
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 380 - 430 °F
Mold Temperature 100 - 125 °F
Drying Temperature 175 °F
@Time 7200 sec
Moisture Content 0.10 %
Injection Pressure 10000 - 15000 psi
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
RTP Company RTP 128 HI Z  Polypropylene (PP) Talc 20% - High Impact - FDA Type
RheTech Products GC20P105-08FA 20% Glass Fiber Reinforced Polypropylene, Chemically Coupled, FDA Compliant, Black
RTP Company RTP 103 Z Polypropylene (PP), Glass Fiber - FDA Compliant Ingredients
LG Chemical LUPOL GP2200 PP+GF20%
Amco PRIMATOP PP HOMO 201NA Injection Molding Polypropylene

PQZUA4171 / 134884

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.