MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DIAB Divilette® 600 Polyester Resin-based Core Bedding Adhesive  (discontinued **)
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyester, TS; Polyester (Thermoset) - Rigid

Material Notes: Divilette is a polyester resin based core bedding adhesive specifically formulated for use with Diab's structural core materials. It is catalyzed with standard MEKP catalyst. Proper use of Divilette ensures all of the cuts in the core are completely filled and that no air entrapment exists between the core and the laminate. It is easy to apply with no run on vertical surfaces. Divilette can be applied with a spray applicator or hand towel.

Divilette must be catalyzed with an MEKP 9% active oxygen content catalyst.
Divilette exhibits less than a 1% linear shrinkage (ASTM D2566).

Information provided by DIAB, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.601 g/cc0.0217 lb/in³
Viscosity 35000 - 54000 cP
@Temperature 22.2 °C
35000 - 54000 cP
@Temperature 72.0 °F
ASTM D1824
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 10.0 MPa1450 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Tensile Modulus 1.00 GPa145 ksiASTM D638
 
Thermal PropertiesMetricEnglishComments
Shrinkage <= 1.0 %<= 1.0 %ASTM D2566
 
Processing PropertiesMetricEnglishComments
Gel Time 30.0 - 45.0 min30.0 - 45.0 minASTM D2471
 
Descriptive Properties
Water Absorption80 oz

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Glass Fiber, Generic
NMG ProCell® PC48 PVC Foam Core
Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties)
DIAB TBR® 6 Multifunctional Polymer Core Material
Overview of materials for Epoxy, Cast, Unreinforced

PDIAB58 / 29833

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.