MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy, M01 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Temper: As Sand Cast

Casting Characteristics: High – Drossing, Shrinkage in Solidification; Medium – Fluidity, Gassing; Low - Casting Yield, Effect of Section Size

Fabrication Properties: Excellent Suitability – Gas Shielded Arc Welding; Good Suitability – Soldering, Brazing, Coated Metal Arc Welding

Typical uses: Safety Tools; Nuts; Stator Clamps; Bushings; Gears; Hot Mill Guides; Impellers; Pickling Equipment; Propellers; Pump Casings; Stator Clamp Segments; Valves; Wear Plates; Welding Rods; Worms; Marine Hardware

Applicable Specifications: As Continuous Cast – ASTM B505/B505M; As Sand Cast – Castings ASTM B148; Ingot – ASTM B30

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.272 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 180
@Load 3000 kg
Tensile Strength >= 90.0 ksifor Standard
 95.0 ksiTypical
Tensile Strength, Yield >= 40.0 ksifor Standard, 0.5% Ext
 45.0 ksiTypical, 0.5% Ext
Elongation at Break >= 20 %for Standard
 26 %Typical
Creep Strength 9600 psi0.1% per 10,000 hours
Rupture Strength 34000 psi
Tensile Modulus 18000 ksi
Modulus of Rigidity 6787 ksiCalculated
Compressive Strength 150 ksi0.1 in. set/in.
Poissons Ratio 0.326
Fatigue Strength 33000 psi
@# of Cycles 1.00e+8
Machinability 50 %
Izod Impact 25.0 ft-lb
Charpy Impact 30.0 ft-lbV-Notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000570 ohm-cm3% IACS
Magnetic Permeability 1.03Annealed, Fast Cooled Condition
 2.2Slow Cooled Condition, Range 2.2 to 15.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.80 µin/in-°F
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.105 BTU/lb-°F
Thermal Conductivity 7.00 BTU-in/hr-ft²-°F
Melting Point 1742 - 1814 °F
Solidus 1742 °F
Liquidus 1814 °F
Shrinkage 1.56 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 600 °FStress Relief
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 7.0 - 8.5 %
Copper, Cu >= 71 %
Iron, Fe 2.0 - 4.0 %
Manganese, Mn 11 - 14 %
Nickel, Ni 1.5 - 3.0 %
Silicon, Si <= 0.10 %
 
Descriptive Properties
Proportional Limit22 ksi
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC95800x3 / 293248

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.