System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Aurora Plastics GA-1046CTLF PVC
Categories:
Polymer
;
Thermoplastic
;
Vinyl (PVC)
;
PVC, Molded
Material Notes:
Application: Lead free 105° C tri-rated semi-rigid insulation compound suitable for UL style 1061, CSA-SRPVC, MIL-I-16878.
Information provided by S&E Specialty Polymers; S&E Specialty Polymers was aquired by Aurora Plastics in 2017.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.29
-
1.35
g/cc
ASTM D792
Mechanical Properties
Original Value
Comments
Hardness, Shore D
67 - 73
ASTM D2240
Tensile Strength
26.5
MPa
ASTM D412
28.35
MPa
@Treatment Temp. 136 °C,
Time 605000 sec
Air Oven aged
Elongation at Break
320 %
ASTM D412
284.8 %
@Treatment Temp. 136 °C,
Time 605000 sec
Air Oven aged
100% Modulus
2.90
ksi
@Strain 100 %
ASTM D412
Electrical Properties
Original Value
Comments
Volume Resistivity
1.80e+14
ohm-cm
ASTM D257
Thermal Properties
Original Value
Comments
Oxygen Index
29 %
ASTM D2863
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Karina 18/387-RG-GE (CS) Gray Color Concentrate for PVC
Colorite Polymers 9904 Clear Extrusion Vinyl Compound
BASF Elastollan® R 2002 25% Glass Filled TPUR
A.D. Compound Adene NCTAG Copolymer 50% CaCO3 Filled Polypropylene
PSEPO021 / 140984
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.