MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
North American Elm Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Good strength, toughness and bending properties Ring-Porous Hardwood. Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Coarse
Dimensional changes when dried lumber is subjected to variations in humidity during service: Medium
Resistance to fungal decay (Heartwood in ground contact): Non-durable (5 to 10 years)
Resistance to penetration by preservatives: Moderately Resistant
Common Applications: Furniture, coffins, rubbing strips

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Ulmus americana; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.460 g/ccOven Dry Weight/Unseasoned Volume
 54.0 lb/ft³Unseasoned*
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 2400 NSide. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 2700 NEnd. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 3700 NSide
Tensile Strength, Ultimate 4.60 MPaPerpendicular to Grain
 560 psiPerpendicular to Grain*
Modulus of Rupture 0.0510 GPaStatic Bending
 6.90 ksiStatic Bending*
Flexural Yield Strength 3600 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 9.20 GPaStatic Bending
 1030 ksiStatic Bending*
Compressive Strength 4.80 MPaPerpendicular to Grain
 38.0 MPaParallel to Grain
 390 psiPerpendicular to Grain*
 2290 psiParallel to Grain*
 2880 psiMax Crushing Strength Parallel to Grain*
Machinability 50 %Medium Relative to Other Wood
Shear Strength 10.4 MPaOrientation Unknown
 920 psiParallel to Grain*
Impact 2.9in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 8100psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.830 in-lb/in³Static Bending*
Work to Maximum Load 11.0 in-lb/in³Static Bending*
Cleavage 37.0 kN/mRadial surface of failure, Unseasoned*
 47.0 kN/mTangential surface of failure, Unseasoned*
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.860 BTU-in/hr-ft²-°FOven Dry
 1.00 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 4.2 %Radial; Green to Zero Moisture
 9.5 %Tangential; Green to Zero Moisture
 14.6 %Volumetric; Green to Zero Moisture
 
Descriptive Properties
ColorPale reddish-brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Maple, Rock (Sugar Maple)
North American Quaking Aspen (Trembling Aspen) Wood
Northern White Pine Wood
American Black Walnut Wood
American Ash Wood

PTSA110 / 71249

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.