MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Medalist® MD-50253 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-50200 Series is a high performance thermoplastic elastomer series, designed to be a sustainable alternative to flexible PVC for medical tubing and film. Medalist MD-50253 is a medium hardness, low density, clear grade, available in NAT and color-matched, intended for use in medical and healthcare applications, with excellent processability and throughput in extruded tubing.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Colorability Good Processability; Good Sterilizability; Halogen Free; High Clarity; High Purity; Low Density; Low Specific Gravity; Medium Hardness; No Animal Derived Components; Radiation (Gamma) Resistant

Uses: Clear Sheet; Film; Hose; Medical/Healthcare Applications; Pharmaceuticals; Rubber Replacement; Tubing

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion; Cast Film

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/ccASTM D792
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 53
@Time 5.00 sec
ASTM D2240
 55
@Time 1.00 sec
ASTM D2240
Tensile Strength at Break 1340 psiASTM D412
Tensile Stress at Strain 220 psi
@Strain 50 %
ASTM D412
 270 psi
@Strain 100 %
ASTM D412
 415 psi
@Strain 300 %
ASTM D412
Elongation at Break 890 %ASTM D412
Tear Strength 177 pliASTM D624
Compression Set 9.1 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Processing Temperature 340 - 380 °FMelt, Injection
Rear Barrel Temperature 260 - 300 °FInjection
Middle Barrel Temperature 280 - 320 °FInjection
Front Barrel Temperature 300 - 340 °FInjection
Nozzle Temperature 340 - 380 °FInjection
Zone 1 340 - 370 °FExtrusion
Zone 2 360 - 385 °FExtrusion
Zone 3 365 - 400 °FExtrusion
Zone 4 365 - 400 °FExtrusion
Zone 5 400 - 440 °FExtrusion
Die Temperature 400 - 440 °FExtrusion
Mold Temperature 70.0 - 100 °FInjection
Injection Pressure 200 - 800 psiInjection
Back Pressure 25.0 - 100 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0735 / 237226

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.