MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Fluorinert™ FC-770 Electronic Liquid
Categories: Fluid

Material Notes: 3M™ Fluorinert™ Liquid FC-770 is a non-conductive, thermally and chemically stable fluid with a wide liquid range (-125 to 95 deg C) for use in many low temperature heat transfer application such as reliability testing and cooling of electronics.

Features and Benefits

  • Thermal stability
  • Chemical stability
  • Wide liquid range
  • Non-conductive
  • Narrow boiling range
  • Compatibility

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.793 g/ccLiquid
Solubility in Water <= 0.00 %
Solubility 14 ppm
Viscosity 1.359 cPAbsolute
Kinematic Viscosity 0.79 cSt
Molecular Weight 399 g/mol
Vapor Pressure 0.0657 bar
Surface Tension 14.8 dynes/cm
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 24.7 barEstimated
Critical Temperature 238 °CCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 3.00e+14 ohm-cmASTM D257
Dielectric Constant 1.9
Dielectric Strength >= 40.0 kV/in0.1" gap
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 85.9 J/gLatent, at normal boiling point
CTE, linear 1480 µm/m-°C
Specific Heat Capacity 1.038 J/g-°CLiquid
Thermal Conductivity 0.0630 W/m-KLiquid
Boiling Point 95.0 °C
@Pressure 0.101 MPa
Pour Point -127 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.27
 
Descriptive Properties
ColorClear, colorless

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
2-Octanol, C8H18O
2-Butoxyethanol, C6H14O2
2-Butanol (CH3CH2CH(OH)CH3; secondary-Butyl Alcohol)
1-Pentanol, C5H12O
1-Octanol, C8H18O

PMM33088 / 167835

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.