MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

303 SE Stainless Steel, annealed
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Short time tensile test

Key Words: T303, T 303, 303Se, 303SS, 303 SS, UNS S30323, AMS 5640 (type 2), AMS 5641, AMS 5738, ASME SA194, ASME SA320, ASTM A194, ASTM A194 (8F), ASTM A314, ASTM A320, ASTM A473, ASTM A581, ASTM A582, MIL SPEC MIL-S-862, SAE J405 (30303 Se), DIN 1.4305, X12CrNiS188, B.S. 303 S 41, EN 58M, austenitic, 18-8
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.00 g/cc0.289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 620 MPa89900 psi
 140 MPa
@Temperature 870 °C
20300 psi
@Temperature 1600 °F
 205 MPa
@Temperature 760 °C
29700 psi
@Temperature 1400 °F
 310 MPa
@Temperature 650 °C
45000 psi
@Temperature 1200 °F
 380 MPa
@Temperature 540 °C
55100 psi
@Temperature 1000 °F
 420 MPa
@Temperature 425 °C
60900 psi
@Temperature 797 °F
Tensile Strength, Yield 240 MPa
@Strain 0.2 %
34800 psi
@Strain 0.2 %
 70.0 MPa
@Strain 0.2 %,
Temperature 870 °C
10200 psi
@Strain 0.2 %,
Temperature 1600 °F
 145 MPa
@Strain 0.2 %,
Temperature 760 °C
21000 psi
@Strain 0.2 %,
Temperature 1400 °F
 205 MPa
@Strain 0.2 %,
Temperature 650 °C
29700 psi
@Strain 0.2 %,
Temperature 1200 °F
 235 MPa
@Strain 0.2 %,
Temperature 540 °C
34100 psi
@Strain 0.2 %,
Temperature 1000 °F
 240 MPa
@Strain 0.2 %,
Temperature 425 °C
34800 psi
@Strain 0.2 %,
Temperature 797 °F
Elongation at Break 50 %50 %in 50 mm
Tensile Modulus 193 GPa28000 ksi
Poissons Ratio 0.250.25Calculated
Shear Modulus 77.2 GPa11200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000720 ohm-cm0.0000720 ohm-cm
Magnetic Permeability 1.0081.008at RT
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.2 µm/m-°C
@Temperature 0.000 - 100 °C
9.56 µin/in-°F
@Temperature 32.0 - 212 °F
 17.8 µm/m-°C
@Temperature 0.000 - 315 °C
9.89 µin/in-°F
@Temperature 32.0 - 599 °F
 18.4 µm/m-°C
@Temperature 0.000 - 540 °C
10.2 µin/in-°F
@Temperature 32.0 - 1000 °F
 18.7 µm/m-°C
@Temperature 0.000 - 650 °C
10.4 µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  16.2 W/m-K
@Temperature 100 °C
112 BTU-in/hr-ft²-°F
@Temperature 212 °F
 21.5 W/m-K
@Temperature 500 °C
149 BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point 1400 - 1420 °C2550 - 2590 °F
Solidus 1400 °C2550 °F
Liquidus 1420 °C2590 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.15 %<= 0.15 %
Chromium, Cr 18 %18 %
Iron, Fe 69 %69 %
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 9.0 %9.0 %
Phosphorus, P <= 0.20 %<= 0.20 %
Selenium, Se <= 0.15 %<= 0.15 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.060 %<= 0.060 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
303 Stainless Steel, annealed
AISI 303 Cast Stainless Steel, ASTM A582
302 Stainless Steel, annealed strip
410 Stainless Steel
416 Stainless Steel

MQ303I / 12664

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.