MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Covestro Makrolon® 1239 Polycarbonate, Blow Molding/Extrusion Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: Pseudoplastic behavior and high viscosity extrusion and injection molding grade, BgVV- and FDA grade for food contact applications, high melt stability, better resistance to hot water, specially suitable for extrusion blow molding.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/cc
Moisture Absorption at Equilibrium 0.15 %50% RH
Water Absorption at Saturation 0.35 %
 0.35 %
Viscosity 800000 cP
@Shear Rate 25 1/s,
Temperature 320 °C
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cmASTM D955
Melt Flow 3.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 124ASTM D785
Tensile Strength, Ultimate 69.0 MPaASTM D638
Tensile Strength, Yield 63.0 MPa
Elongation at Break 110 %ASTM D638
Elongation at Yield 6.0 %
Tensile Modulus 2.40 GPa
Flexural Yield Strength 85.0 MPaat 5% strain; ASTM D790
Flexural Modulus 2.30 GPaASTM D790
Izod Impact, Notched 9.10 J/cm
@Thickness 3.20 mm
ASTM D256
Charpy Impact Unnotched NB
Tensile Creep Modulus, 1 hour 2200 MPa
Tensile Creep Modulus, 1000 hours 1900 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity >= 1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
Dielectric Constant 2.9
@Frequency 1e+6 Hz
 3.0
@Frequency 100 Hz
Dielectric Strength 30.0 kV/mm
Dissipation Factor 0.0010
@Frequency 100 Hz
 0.010
@Frequency 1e+6 Hz
Arc Resistance 120 secTungsten Electrodes; ASTM D495
Comparative Tracking Index 275 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 1.17 J/g-°CASTM D2766
Thermal Conductivity 0.200 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
Vicat Softening Point 147 °C
Glass Transition Temp, Tg 148 °C
UL RTI, Electrical 75.0 °C
UL RTI, Mechanical with Impact 75.0 °C
UL RTI, Mechanical without Impact 75.0 °C
Oxygen Index 26 %
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586
Haze 1.0 %
@Thickness 3.17 mm
ASTM D1003
Transmission, Visible 87 %
@Thickness 3.20 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 280 - 320 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Inovyn 258RD Polyvinyl Chloride General Purpose - Rigid
Covestro Makrolon® WB1239 Polycarbonate
Covestro Apec® 1800 Polycarbonate
Envalior Akulon® K240-HP PA6-I, Conditioned, Heat Stabilized, Impact Modified, Extrusion Blow Molding
LG Chemical Lupoy 1603-03 Polycarbonate Resin

PBA426 / 26927

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.