MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

PTS PBT-6630 30% Glass Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: PBT6630 is an injection molding grade, with 30% glass fiber reinforced, high heat stability, and electrical properties, easy to process. It is widely used in automotive, home appliance, Electrical industry, such as connector, gear housing, and other structural parts.

Information provided by PTS LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.53 g/cc1.53 g/ccISO 1183
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 250 °C
13 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 123 MPa17800 psiISO 527-2/1
Elongation at Break 3.1 %3.1 %ISO 527-2/1
Tensile Modulus 9.01 GPa1310 ksiISO 527-2/1A
Flexural Strength 189 MPa27400 psiISO 178
Flexural Modulus 9.25 GPa1340 ksiISO 178
Izod Impact, Notched (ISO) 7.50 kJ/m²3.57 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 202 °C396 °FISO 75-1/-2
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 240 - 260 °C464 - 500 °F
Melt Temperature 230 - 260 °C446 - 500 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 120 - 140 °C248 - 284 °F
Dry Time 3 - 4 hour3 - 4 hour
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
 
Descriptive Properties
Processing Screw SpeedMedium-Fast

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Orgalloy® RS 6030 NAT Polyamide 6 Alloy 30% Glass Fiber reinforced
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
PTS PBT-30GF 30% Glass Fiber Reinforced PBT
PTS PCA-3015 Low Temperature Impact PC/PBT Alloy

PZ9PU936 / 135393

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.