MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Johnson Matthey JM5050 Soft Solder/Flux
Categories: Metal; Nonferrous Metal; Lead Alloy; Solder/Braze Alloy; Tin Alloy

Material Notes: General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materials can be offered as solid wires or as flux cored, to suit the required applications. A wide range of Silver containing solders are suitable for applications where higher strength, increased corrosion resistance or electrical conductivity are required.

In some markets the use of Lead or Cadmium containing solders is prohibited in potable water systems, this has led to the increase use of the Silver bearing and Copper bearing-Lead free solders. Solders are available as: Sticks wire (solid or flux cored), preforms, ingots, ribbon bars and solder paste.


Federal Specification QQ-S-571 50B
ASTM Grade Sn 50
BS.EN 29453 Alloy No. 3

Information provided by Johnson Matthey.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 183 - 216 °C
Solidus 183 °C
Liquidus 216 °C
 
Component Elements PropertiesOriginal ValueComments
Lead, Pb 50 %
Tin, Sn 50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow Tin 60/Lead 39/Antimony 1 Alloy
Johnson Matthey 95A Lead-Free Soft Solder Alloy
Johnson Matthey JM 97C Soft Solder/Flux
Johnson Matthey JM 99C Soft Solder/Flux
Johnson Matthey JM P35 Soft Solder/Flux

NJMMJ33 / 17639

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.