MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CIMBAR RiverCal™ 8107 & 8107C Calcium Carbonate (CaCO3)
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: RiverCal™ 8100 Series Calcium Carbonate are high purity, white, functional fillers targeted for use in thermosets, thermoplastics, paint & coatings, sealants, TPO's and TPE's and other applications requiring an economical filler. RiverCal™ 8100 Series products are also available with stearic acid surface coating, designated with a "C", where improved flow and reduced dusting are required.

Information provided by Cimbar Performance Minerals.

Key Words: CaCO3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.71 g/cc
Bulk Density 36.0 lb/ft³Loose
 87.0 lb/ft³Tapped
Brightness 89 %Stearate Treated, Hunter Rd value
 92 %Uncoated, Hunter Rd value
Oil Absorption 15 %g oil/100 g filler; ASTM D281
Fineness 5.0Hegman Fineness; ASTM D1210
Moisture Absorption at Equilibrium 0.30 %
Loss On Ignition 44 %
@Temperature 1050 °C
Particle Size 1.8 µm@ 10%
 5.0 µmD50
 32 µm@ 98%
Particle Mesh Size 325 Mesh0.5% retained
pH 9.5
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 <= 0.10 %
 
Descriptive Properties
CaCO399
MgCO3< 1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CIMBAR Crescent 12 Calcium Carbonate (CaCO3), Fine Powder
CIMBAR Crescent 50 Calcium Carbonate (CaCO3), Coarse Powder
CIMBAR Crescent 35 Calcium Carbonate (CaCO3), Medium Powder
Excalibar ExCal® CW 325 Calcium Carbonate CaCO3 Powder
Calcium Carbonate, Calcite (CaCO3)

CIMBAR953 / 133435

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.