Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: Food Contact Acceptable; Medium Viscosity Uses: Cast Film; Consumer Applications; Film; Industrial Applications; Medical Devices; Medical/Healthcare Applications; Non-oriented Film; Packaging Agency Ratings: EU Food Contact; FDA Food Contact; USP Class VI RoSH Compliance: RoSH Compliant Appearance: Natural Color Forms: Granules Processing Method: Cast Film; Extrusion; Film Extrusion; Injection Molding Information provided by EMS-Grivory |