MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE ME-1360N-01 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-1360N-01 is a general purpose thermoplastic elastomer used in automotive applications. Sarlink ME-1360N-01 is a medium hardness, low density, lubricated grade exhibiting superior compression set and chemical resistance. This grade can be processed by injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: General Purpose; Good Colorability; Good Flow; Good Moldability; Good Processability; Low Density; Medium Hardness; Low Specific Gravity; Slip; Lubricated; Medium Flow

Uses: Automotive Applications; Automotive Interior Parts; General Purpose; Grommets

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D792
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 61Injection Molded; ASTM D2240
 57
@Time 15.0 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 680 psiFlow; ASTM D412
 1380 psiAcross Flow; ASTM D412
Tensile Stress at Strain 220 psi
@Strain 100 %
Across Flow; ASTM D412
 310 psi
@Strain 100 %
Flow; ASTM D412
Elongation at Break 620 %Flow; ASTM D412
 900 %Across Flow; ASTM D412
Tear Strength 156 pliAcross Flow; ASTM D624
Compression Set 23 %
@Temperature 22.8 °C,
Time 79200 sec
ASTM D395
 38 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 88 %
@Temperature 125 °C,
Time 252000 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 390 - 410 °F
Middle Barrel Temperature 400 - 420 °F
Front Barrel Temperature 410 - 430 °F
Nozzle Temperature 420 - 440 °F
Melt Temperature 420 - 440 °F
Mold Temperature 60.0 - 90.0 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 125 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 120 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1051 / 237542

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.