MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® Nuva-Sil® 5084 Sealant
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes:
Silicon Light Cure Adhesives and Gasketing and Wire Tackers
Loctite® innovative gasketing products offer precise, reliable sealing of electronic enclosures, protecting them from environmental hazards. Loctite offers both Form-in-place (FIP) and Cure-in-Place (CIP) compression gasket materials.

Loctite® Tak Pak Adhesives are used to secure wires to printed circuit board assemblies. The fast cure times of these adhesives help increase the throughput of the wire tacking assembly process.

Loctite® 5084 Form-In-Place Nuva-Sil® Sealant
A one part non-corrosive form-in-place silicone sealant that provides severe environmental protection. UV cure allows parts to be sealed in seconds. Secondary moisture cure ensures full cure, even in shadowed areas. Key Substrates: Glass, Metal, Ceramic Cure Type: Ultraviolet, Moisture, Methoxy Bonding Type: Silicone UL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 150 cP
@Temperature 25.0 °C
Extrusion rate, grams/minute, 1/8" orifice at 90 psi
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 45
Tensile Strength, Ultimate 550 psi
Elongation at Break 200 %
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °F
Minimum Service Temperature, Air -65.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 secat 75 mW/cm^2
 
Descriptive Properties
ColorYellow/Transparent
Extrusion Rate150 g/min1/8" orifice at 90 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® Output™ 5404 Heat Cure Silicone
Henkel Loctite® 5420 Heat Cure Form-In-Place Electrically Conductive Silicone Sealant
Momentive Performance Materials TSE322B Heat-Curing Silicone Adhesive, Black
Momentive Performance Materials TSE326 High Temperature, Heat Cured One Component Silicone Adhesive
Henkel Loctite® 5920™ RTV Silicone Sealant

PLOCT188 / 51924

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.