MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Radici RADILON® MIXLOY D CPA100K 100 NT PA610/ABS Blend, 10% Mineral Reinforced, Conditioned
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend

Material Notes: Description: PA610/ABS blend, 10% mineral filled injection molding grade. Heat stabilized. Natural color. Suitable for parts requiring good dimensional stability and low warpage. Improved impact resistance and very good property retention after moisture absorption.

Processing: Injection Molding

Delivery Form: Granules

Additives: Release agent

Special Characteristics: Heat stabilized or stable to heat, Amorphous, Improved Dimensional Stability, High Surface Aspect, Low Moisture Absorption

Industries: Automotive, Consumer Industry Goods, Transportation

Regional Availability: North America, Europe, Asia Pacific, South and Central America, Near East/Africa

Information provided by Radici Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³ISO 1183
Water Absorption 2.3 %
@Thickness 2.00 mm
2.3 %
@Thickness 0.0787 in
Immersion at 23°C; ISO 62
Moisture Absorption 0.800 %
@Thickness 2.00 mm
0.800 %
@Thickness 0.0787 in
50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 40.0 MPa5800 psi50 mm/min; ISO 527-2/1A
Elongation at Break 80 %80 %Nominal, 50 mm/min; ISO 527-2/1A
Elongation at Yield 25 %25 %50 mm/min; ISO 527-2/1A
Tensile Modulus 1.60 GPa232 ksi1mm/min; ISO 527-2/1A
Flexural Strength 55.0 MPa7980 psi2mm/min; ISO 178
Flexural Modulus 1.80 GPa261 ksi2mm/min; ISO 178
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 1.60 J/cm²7.61 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 223 °C433 °FISO 11357-1/-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 40.0 - 60.0 °C104 - 140 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADICI096 / 313597

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.