MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASI® Threadlocker TORQUE 42 TL Anaerobic Solid Polyacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: ADVANCED PERFORMANCE SERIES THREADLOCKER 42TL is a thixotropic anaerobic compounds formulated to cure rapidly and reliably on most “as received” fasteners. They give predictable lubricity on assembly. Typical Applications: LOCKING AND SEALING, Hydraulic Line Fittings, Vacuum cleaner bell housing screws, Hydraulic pistons nuts, Rocker Nuts, Oil pressure switch assembly, Construction equipment bolts, Bulldozers track bolts, Railroad bolts on wear plates, Typewriter screws, Carburetor adjusting screws, Machinery Keys.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/ccuncured
Viscosity 1200 cP1200 cPuncured
 
Mechanical PropertiesMetricEnglishComments
Shear Strength 5.50 MPa798 psicured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °F
Minimum Service Temperature, Air -53.9 °C-65.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 10.0 - 30.0 min0.167 - 0.500 hour20% Fix (1)
 
Descriptive Properties
Bolt Treating RangeUncured. 1/4 to 3/4 in
Chemical ClassSolid Polyacrylate
Color / appearanceBlue. Uncured & cured
CorrosivityNone. Uncured. MIL (S-46163-A) Type II Grade N

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASINC9173 / 233539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.