MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SSAB Tunnplat Domex® 024 BOR Water quenched Boron Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel

Material Notes: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Compared to conventional quenched and tempered steels, boron steel have several benefits including better formability. Boron steels are used for a wide variety of applications - as a wear material and as a high-strength structural steel. Examples include wear plate, screen plate, punching tools, spades, knives, saw blades, caterpillar tracks, and agricultural machinery.

Data provided by SSAB Tunnplat.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.87 g/ccEstimated by MatWeb
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 490HV10; approximate
Tensile Strength, Ultimate 1600 MPa
Tensile Strength, Yield 1200 MPa
Elongation at Break 10 %A5
Impact 25J/cm²; -20°C
 35J/cm²; 20°C
 
Component Elements PropertiesOriginal ValueComments
Boron, B 0.0030 %
Carbon, C 0.20 - 0.25 %
Chromium, Cr 0.15 - 0.25 %
Iron, Fe 98 %As Remainder
Manganese, Mn 1.0 - 1.3 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.20 - 0.35 %
Sulfur, S <= 0.025 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SSAB Tunnplat Docol® 1200 DP High-strength Steel
SSAB Tunnplat Domex® 014 BOR Oil quenched Boron Steel
SSAB Tunnplat Domex® 044 BOR Water quenched Boron Steel
SSAB Tunnplat Domex® 014 BOR Rolled Boron Steel
SSAB Tunnplat Domex® 024 BOR Oil quenched Boron Steel

NTUNN85 / 19577

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.