MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
MBA Polymers HDPE 1107 E Post-consumer recycled fractional melt high density polyethylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Available in standard black.

Information provided by MBA Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccMBA Method
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 20.0 MPa
@Temperature 23.0 °C
ISO 527-2/50
Flexural Modulus 600 MPa
@Temperature 23.0 °C
ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
 
Processing PropertiesOriginal ValueComments
Melt Temperature 190 - 210 °CInjection Molding Range
 200 °CRecommended Injection Molding
 190 - 210 °CExtrusion Range
 200 °CRecommended Extrusion
Mold Temperature 10.0 - 30.0 °C
 20.0 °CRecommended
Drying Temperature 70.0 °C
@Time 3600 - 7200 sec
Moisture Content <= 0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem BT 003 HDPE Blow Molding Polyethylene
Braskem Green PE SHC7260 Injection Molding High Density Polyethylene
Forever Plast Namtene® Recycled Standard HDPE
RTP Company RTP 799 X 140537 High Density Polyethylene (HDPE); Cellulose Fiber - 95% Renewable Resource Content
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene

PMBAP997 / 161704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.