MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Nouryon Trigonox 301-CM25 3,6,9-Triethyl-3,6,9-trimethyl-1,4,7-triperoxonane, solution in isoparaffinic hydrocarbons
Categories: Other Engineering Material

Material Notes: Trigonox 301-CM25, solution in isoparafinnic hydrocarbons, is an initiator for the production of controlled rheology polypropylene (CR-PP) and high temperature polymerization of ethylene.

CAS number: 24748-23-0

EINECS/ELINCS No: 429-320-2

Applications: Trigonox 301-CM25 is an efficient peroxide formulation for the production of controlled rheology polypropylene (CR-PP) in an extrusion process. An important advantage of Trigonox 301-CM25 is that the final CR-PP contains a low content of volatiles originating from peroxide decomposition products. Trigonox 301-CM25 forms no acetone and no tert butanol.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.841 g/cc
Half-life 0.100
@Temperature 170 °C
[hr]
 1.00
@Temperature 146 °C
[hr]
 10.0
@Temperature 125 °C
[hr]
Viscosity 2.25 cP
Molecular Weight 264.3 g/mol
Storage Temperature 0.000 - 40.0 °C
 
Thermal PropertiesOriginal ValueComments
Decomposition Temperature 90.0 °CSelf-Accelerating Decomposition Temperature
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
AppearanceClear to slightly hazy liquid
Content3.6 - 4.9 %Total active oxygen
Content (%)18.16Active oxygen content peroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY1103 / 286626

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.