MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

E-Polymers SEPAZ® LH40 PP Homopolymer LFT Resin
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and delivers optimal reinforcement to the plastic matrix in contrast to conventional short glass fiber-reinforced thermoplastics. Molded parts made of SEPAZ LFT are used in virtually every sector of consumer and industrial manufacturing, including automotive, recreation & sports, marine, food & beverage.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.21 g/cc1.21 g/ccASTM D792
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 117.72 MPa17074 psiASTM D638
Elongation at Break 2.5 %2.5 %ASTM D638
Flexural Strength 181.49 MPa26323 psiASTM D790
Flexural Modulus 8.3385 GPa1209.4 ksiASTM D790
Izod Impact, Notched  2.94 J/cm
@Temperature 23.0 °C
5.51 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 2.94 J/cm
@Temperature -30.0 °C
5.51 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FASTM D648
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 215 - 225 °C419 - 437 °F
Mold Temperature 40.0 - 70.0 °C104 - 158 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUPOL GP-3152F General Purpose Polypropylene, 15% Mineral Fillers, High Impact, Flame Retardant
Cossa Polimeri ESTAPROP HK 2540 T8 Polypropylene, 20% Mineral Filled
Cossa Polimeri ESTAPROP H 1280 T8 Polypropylene, 40% Mineral Filled
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Dry)

PEPOLZ082 / 103579

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.