MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Solvay VTA® 260 Adhesive Film
Categories: Polymer; Adhesive; Film

Material Notes: Description: VTA®260 is a variable cure temperature film adhesive suitable for bonding both composite substrates and aluminum to themselves or to honeycomb and foam core materials. VTA260 is fully cure compatible with Cytec’s VTM pregreg range.

Features & Benefits:

  • 30 days out life at 21°C (70°F)
  • 12 months storage at -18°C (0°F)
  • Flexible cure between 65 and 120°C (149 and 248°F)
  • Minimum cure temperature 65°C (149°F)
  • Good tack for easy lay-up of large structures, vertical surfaces and complex shapes
  • Maximum dry service temperature of 120°C (248°F) after full post-cure

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccCured Resin
Storage Temperature -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 870 psi
@Temperature 80.0 °C
Lap, 16 hrs at 65°C, Material: PK13-313g/m3; ASTM D3165-00
 2180 psi
@Temperature 120 °C
Lap, 1 hr at 120°C, Material: PK13-313g/m3; ASTM D3165-00
 2320 psi
@Temperature 80.0 °C
Lap, 5 hrs at 80°C, Material: PK13-313g/m3; ASTM D3165-00
 3340 psi
@Temperature 21.0 °C
Lap, 16 hrs at 65°C, Material: PK13-313g/m3; ASTM D3165-00
 3770 psi
@Temperature 80.0 °C
Lap, 1 hr at 120°C, Material: PK13-313g/m3; ASTM D3165-00
 4350 psi
@Temperature 21.0 °C
Lap, 5 hrs at 80°C, Material: PK13-313g/m3; ASTM D3165-00
 5510 psi
@Temperature 21.0 °C
Lap, 1 hr at 120°C, Material: PK13-313g/m3; ASTM D3165-00
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °Cfor cure 5 hrs at 80°C
 110 °Cfor cure 2 hrs at 100°C
 120 °Cfor cure 1 hrs at 120°C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 120 °C
 2.00 hour
@Temperature 100 °C
 5.00 hour
@Temperature 80.0 °C
Shelf Life 12.0 Month
 
Descriptive Properties
ColorPink

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elantas Conap FR-1046 / EA-02 Conapoxy® Resin / Conacure® Hardener
Solvay FM® 377S Adhesive Film, psf 0.06 (293 gsm)
Solvay VTF 261 Film
Solvay Thornel® T-605/50X 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Solvay Thornel® T-40 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor

PCYTED109 / 180411

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.