MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ITW Plexus® MA2045 Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Plexus® MA2045 is a two-part methacrylate adhesive designed for structural bonding of composite, thermoplastic, and metal assemblies. MA2045 was uniquely formulated to eliminate problems associated with adhesive sag and slide, even when applied to a vertical surface. In addition, MA2045 does not boil in gaps up to 1.5 inches thick. Combined at a 10:1 ratio at 75°F (24°C), it has a working time of approximately 50 minutes and achieves 500 psi and 1000 psi in approximately 100 and 130 minutes, respectively. As with most other Plexus methacrylate systems, MA2045 requires little-to-no surface preparation. MA2045 provides a unique combination of excellent fatigue endurance, outstanding impact resistance, and superior toughness. MA2045 is supplied in 380-ml cartridges, 5-gallon (20-liter) pails, or 50-gallon (200-liter) drums to be dispensed as a non-sagging gel.

Excellentl resistance to: ? Hydrocarbons ? Acids and Bases (pH 3-10) ? Salt Solutions Susceptible to: ? Polar Solvents ?Strong Acids and Bases. Recommended for: ? ABS ? Acrylics ? FRP ? Gel coats ? PVC ? Polyesters (including DCPD modified) ? Select metals ? Styrenics ? Urethanes (general) ? Vinyl Esters

Plexus Primer ( Exterior applications require the use of coatings or primers that inhibit oxidation of the steel.) Adhesive color: off white ( uncured-room temperature). Activator color: blue/black (uncured-room temperature).

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.942 g/cc0.0340 lb/in³adhesive. Uncured.
 0.953 g/cc0.0344 lb/in³Cured
 1.07 g/cc0.0385 lb/in³Activator. Uncured.
Volatile Organic Compounds (VOC) Content <= 10 g/l<= 10 g/lDuring cure
Viscosity  35000 - 70000 cP
@Temperature 22.2 °C
35000 - 70000 cP
@Temperature 72.0 °F
Activator
 180000 - 220000 cP
@Temperature 22.2 °C
180000 - 220000 cP
@Temperature 72.0 °F
Adhesive
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 15.2 - 20.0 MPa2200 - 2900 psiASTM D638
Elongation at Break 90 - 125 %90 - 125 %ASTM D638
Tensile Modulus 0.414 - 0.689 GPa60.0 - 100 ksiASTM D638
Adhesive Bond Strength 11.0 - 15.2 MPa1600 - 2200 psiLap Shear Cohesive Strength; ASTM D1002
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 82.2 °C180 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flash Point 10.6 °C51.0 °F
 
Processing PropertiesMetricEnglishComments
Working Life 40.0 - 50.0 min
@Temperature 23.3 °C
40.0 - 50.0 min
@Temperature 74.0 °F
Shelf Life 10.0 Month10.0 MonthCartridges
 10.0 Month10.0 MonthActivator (B side)
 13.0 Month13.0 MonthAdhesive (A side)
 
Descriptive Properties
Fixture Time (mins)100 to 13074°F cure. Varies with bond gap and temperature.
Gap Filling (in)0.03 to 1.5Room temperature cure.
Mix Ratio by volume10 to 1Adhesive to Activator. Room temperature
Mix Ratio by weight8.83 to 1.0Adhesive to Activator. Room temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWP9010 / 239520

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.