MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kaltun COATTUN MICA SMW.245 Paint/Coating Additive
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: COATTUN mica is used in architectural and industrial paints and coatings and they enhance their mechanic and optic features. All COATTUN products are produced in mines belonging to Kaltun Madencilik A.S. and located in Çine-Milas region.

Information provided by KALTUN MINING

Key Words: Product Code: KMB.02.M.0045
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.350 g/cc0.0126 lb/in³
Density 2.85 g/cc0.103 lb/in³
Oil Absorption 66 %66 %ISO 787-5
Moisture Absorption 0.300 %0.300 %
Loss On Ignition 3.7 %3.7 %
Particle Size 10.5 µm10.5 µmD10, Laser Diffraction - MIE (Malvern)
 41.5 µm41.5 µmD50, Laser Diffraction - MIE (Malvern)
 155 µm155 µmD97, Laser Diffraction - MIE (Malvern)
 >= 300 µm>= 300 µm0% Screening (wet/dry)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 2.52.5
 
Component Elements PropertiesMetricEnglishComments
Al2O3 27.67 %27.67 %
CaO 0.36 %0.36 %
Fe2O3 1.03 %1.03 %
K2O 8.52 %8.52 %
MgO 1.62 %1.62 %
Na2O 1.36 %1.36 %
P2O5 0.23 %0.23 %
SiO2 55.18 %55.18 %
TiO2 0.34 %0.34 %
 
Descriptive Properties
Color0.3a; Spectrophotometer D65/10°
 4.8b; Spectrophotometer D65/10°
 92.2L; Spectrophotometer D65/10°

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKALT889 / 318187

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.