MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Graft Polymer GRAFTAPOR™ LL-S 02050 Porous Linear Low Density Polyethylene Carrier
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: GRAFTAPOR™ LL-S is a porous polymer carrier for additives, made from LLDPE resin. It’s mainly designed to act as a carrier for additives that are harder to dose during polymer compounding.

Applications:

  • GRAFTAPOR™ LL-S is used to make polymer compounding easier, by absorbing liquid, powder, low melting or thermally sensitive additives.
  • Can absorb solid or paste additives, with melting point up to 40°C below the melting point of GRAFTAPOR™ LL-S.
Supplied as: Granulate.

Properties can be regulated to customer needs.

Information provided by Graft Polymer LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.500 g/ccISO 1183
Porosity 50 %
Pore Size 30.0 microns60% less than 30 µm
 75.0 microns90% less than 75 µm
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 120 °CISO 11357-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis Flexirene® MR 50 U Linear Low Density Polyethylene
Teknor Apex Sinpolene MBW1791 Linear Low Density Polyethylene
Teknor Apex Sinpolene MBW0141 Linear Low Density Polyethylene
ICO Polymers ICOFLO™ 510-5069 400 Micron LLDPE Powder
ExxonMobil LLDPE LL 6101XR Linear Low Density Polyethylene Resin (European Grade)

PGRAFT902 / 232333

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.