MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

IDI Composites E-208 Thermoset Polyester SMC
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: UL Yellow Card SMC

Information provided by IDI Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.70 - 1.90 g/cc1.70 - 1.90 g/ccASTM D792
Water Absorption 0.15 %
@Time 86400 sec
0.15 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 30 - 5030 - 50ASTM D2583
Tensile Strength 124 MPa18000 psiASTM D638
Flexural Strength 234 MPa33900 psiASTM D790
Flexural Modulus 13.8 GPa2000 ksiASTM D790
Compressive Strength 207 MPa30000 psiASTM D695
Izod Impact, Notched 10.7 J/cm20.0 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 12.4 kV/mm315 kV/inASTM D149
Arc Resistance 180 sec180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FASTM D648
Flammability, UL94 V-0
@Thickness 2.00 mm
V-0
@Thickness 0.0787 in
Shrinkage 0.00 - 0.0020 %0.00 - 0.0020 %ASTM D955
 
Descriptive Properties
Bulk Factor App.1ASTM D1895

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PIDI920 / 249310

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.