MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Momentive Performance Materials GE Sealants & Adhesives Advanced Silicone 2 Kitchen & Bath Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: Advanced Silicone 2 Kitchen & Bath sealant is 100% waterproof with 10-year mold-free product protection. Ready for water exposure in as little as 30 minutes, it is ideal for kitchen and bath sealing projects where moisture and humidity may be present. This high-performance durable sealant is permanently flexible with excellent adhesion. Advanced Silicone Kitchen & Bath sealant is neutral curing, which means it is low in odor and will not blemish most metal finishes. Backed by a lifetime guarantee.

Features: Meets ASTM C-920 Class 35 specifications. 40% more flexibility than Class 25 sealants. 5X stronger adhesion than Silicone 1 sealant. Resist mold with 10-year mold-free product protection. 30-minute water-ready. 100% silicone is 100% waterproof. Will not discolor most high-end metal finishes such as chrome, bronze and nickel. Neutral cure with low odor. Permanently flexible. Shrink-proof & crack-proof. Excellent adhesion for wet and dry applications. Freeze/thaw stability. Non-paintable.

Applications: Advanced Silicone 2 Kitchen & Bath sealant is used in a wide variety of applications including showers, tubs, sinks, tile, countertops and fixtures, as well as other kitchen and bath applications.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccCured.
Volatile Organic Compounds (VOC) Content <= 28 g/l<= 28 g/lUncured. Excluding water & exempt compounds; WPSTM C1454
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1515ASTM D2240
Tensile Strength 1.00 MPa145 psiASTM D412
Elongation at Break 347 %347 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -51.1 °C-60.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hourFull Cure
Tack-Free Time 30.0 min0.500 hour50% RH; ASTM C679
Working Life 5.00 - 10.0 min5.00 - 10.0 min
 
Descriptive Properties
AppearancePaste
Carb Chem Curing VOC< 3.0 wt%
ColoralmondGE5060, GE286
 clearGE5040, GE284
 whiteGE5070,GE281
Consistency / Sag< 0.2 inchesASTM D2202
Joint Movement Capability+25% Mortar, AluminumASTM C719.
 ±35% GlassASTM C719.
OdorLight Ammonia
Rain Ready30 minutes
UV & Weathering ResistanceExcellent30 yr study

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9942 / 265753

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.