MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Metallyte™ 70 MET-HB OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: A vacuum-metallized, high barrier OPP film with a proprietary sealant layer. This film offers excellent moisture and oxygen barriers, hot tack, seal integrity, and lap seal range when used with a coextruded outer web. MET-HB is designed specifically for adhesive and extrusion laminations. MET-HB resists crazing in extrusion laminations.

Availability: Latin America, North America and South America

Key Features:

  • Good oxygen barrier
  • Low MST, broad seal range, strong seals
  • High adhesion of aluminum to film
  • Resists crazing in extrusion laminations
  • Excellent hot tack
Features:
  • In Lamination Lap Sealable
  • Light Barrier
  • Moisture Barrier
  • Oxygen Barrier
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Crisps and Snacks
Uses:
  • HFFS Flexible Packaging
  • Pre-made Bags – Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Inner Web Adhesive Lamination, Inner Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 0.190 g/m²/day
@Temperature 38.0 °C
90% RH; ExxonMobil Method
Oxygen Transmission Rate 26.0 cc/m²/day23°C, 0% RH; ExxonMobil Method
Thickness 0.700 milExxonMobil Method
Coating Weight 9.80 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Break, MD 22000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 34000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 4.5 %
@Temperature 135 °C
ExxonMobil Method
Shrinkage, TD 2.5 %
@Temperature 135 °C
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Optical Density 2.4ExxonMobil Method
Transmission, Visible 0.40 %ExxonMobil Method
 
Descriptive Properties
Crimp Seal MST185°F
Crimp Seal Strength400 g/in205°F, 20psi, 3/4sec
Yield44000 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEXB449 / 37754

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.