Product Description: Enflex V1064A BLK UV (thermoplastic vulcanizate) is a fully weatherable black EDPM/PP compound. It is designed to replace thermoset elastomers such as EPDM or polychloroprene, and traditional thermoplastic TPVs. Enflex V grades provide the performance of vulcanized rubber with the advantage of low-cost thermoplastic processing. Availability: North America Features: Acid Resistant; Alcohol Resistant; Base Resistant; Detergent Resistant; Good Processability; Good Weather Resistance; High Heat Resistance; Low Compression Set; Oil Resistant; Ozone Resistant; Recyclable Material; Solvent Resistant; UV Resistant Appearance: Black Processing Method: Extrusion; Injection Molding Information provided by Entec Polymers |