Notes: Medalist MD-17340 is a high performance thermoplastic elastomer specifically designed for healthcare and medical applications. Medalist MD-17340 is a low hardness, low density, halogen-free grade that can be sterilized and is suitable for injection molding, extrusion, and cast film. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Melt Strength; Good Printability; Good Processability; Good Sterilizability; Good Toughness; Halogen Free; Low Density; Low Hardness; Low Odor; Low Specific Gravity; Puncture Resistant; Radiation Sterilizable; Resilient; Slip; Without Fillers Uses: Dental Applications; Film. Hospital Goods; Medical Devices; Medical/Healthcare Applications; Pharmaceuticals; Rubber Replacement Agency Ratings: ISO 10993 Part 5; ISO 13485 RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Cast Film; Film Extrusion; Injection Molding Information provided by Teknor Apex |