MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Yuyao Zhonga ST-06 Nylon 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: It’s used for sports goods, sports equipment, industry electrical apparatus, complete set of switch, industry parts, electric tool, hardware industry, automotive parts, furniture parts, electrical appliances parts, vidicon parts, etc

special purpose: Increase level pliable but strong

Information provided by Yuyao Zhongfa Engineering Plastics CO., LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ASTM D792
Linear Mold Shrinkage 0.015 cm/cm0.015 in/inASTM D955
Melt Flow 10.5 g/10 min10.5 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 60.0 MPa8700 psiASTM D638
Elongation at Break 100 %100 %ASTM D638
Flexural Strength 81.0 MPa11700 psiASTM D790
Flexural Modulus 1.50 GPa218 ksiASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 235 - 265 °C455 - 509 °FInjection Temp
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 85.0 - 90.0 °C185 - 194 °F
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hour
Injection Pressure 60.0 - 100 MPa8700 - 14500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PYUYZ046 / 281839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.