Initiator (30% active ingredient in odorless mineral spirits) for (co)polymerization of vinyl chloride and vinylidine chloride. Highly active initiator developed for the low-temperature polymerization of vinyl chloride to produce high K-value PVC. CAS number: 3437-84-1 EINECS/ELINCS No: 222-340-0 Applications: Trigonox 187-C30 is a highly active initiator especially developed for the low temperature polymerization of vinyl chloride to produce high K-value PVC. Trigonox 187-C30 can also be used in combination with other peroxides such as Di(4-tertbutylcyclohexyl) peroxydicarbonate (Perkadox 16) to increase reactor efficiency. Information provided by Nouryon |