MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Premix Thermoplastics PRE-ELEC® PP 1372  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: PRE-ELEC PP 1372 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PP 1372 has an excellent balance of mechanical properties and is easy to injection mould.

Typical applications include injection molded crates, boxes and tote bins for electronic components and other static sensitive devices (SSD).

Test Specimen - 4.0 mm thick, 10.0 mm wide molded rod.

Information provided by Premix Thermoplastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.980 g/cc
Linear Mold Shrinkage 0.012 - 0.014 cm/cmISO 294-4
Melt Flow 0.60 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 4.0 g/10 min
@Load 5.00 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 96ISO 868
Hardness, Shore D 71ISO 868
Tensile Strength, Ultimate 18.0 MPaISO 527
Tensile Strength, Yield 26.0 MPaISO 527
Elongation at Break 66 %ISO 527
Elongation at Yield 11 %ISO 527
Modulus of Elasticity 1.20 GPaISO 178
Izod Impact, Notched 453 J/m
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180
Izod Impact, Unnotched NB
@Thickness 4.00 mm,
Temperature 23.0 °C
ISO 180
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 1000 ohm-cmISO D-257
Surface Resistance <= 10000 ohmISO D-257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CISO 75/Method Bf
Vicat Softening Point 150 °CRate A; ISO 306/A50
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 250 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 60.0 - 80.0 °C
@Time 7200 - 14400 sec
Pre-drying
Moisture Content <= 0.15 %When Produced
Injection Pressure 8700 - 11600 psi
Shelf Life 12.0 MonthNormal Storing Conditions
 
Descriptive Properties
AppearanceGranule
ColorBlack
Injection SpeedModerate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPREMA049 / 58062

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.