MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Daplen™ ED230HP Polypropylene TPO Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Daplen™ ED230HP is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and gives a good surface quality. Applications: body panels and tailgates.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Linear Mold Shrinkage 0.0010 cm/cmpost shrinkage (2h/90°C)
 0.0080 cm/cmmold average
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 43.0 MPa10N/132 s; ISO 2039
Tensile Strength, Yield 19.5 MPa50mm/min; ISO 527-2
Elongation at Break 100 %50mm/min; ISO 527-2
Elongation at Yield 4.5 %50mm/min; ISO 527-2
Tensile Modulus 1800 MPa1mm/min; ISO 527-2
Flexural Strength 28.0 MPaISO 178
Flexural Modulus 1900 MPa2mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
@Temperature -20.0 °C
ISO 180/1A
 34.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 96.0 kJ/m²ISO 179/1eU
 NBISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 4.00 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 30.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 52.0 µm/m-°C
@Temperature -30.0 - 80.0 °C
Borealis Method
Deflection Temperature at 0.46 MPa (66 psi) 105 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °CISO 75-2
Vicat Softening Point 49.0 °C
@Load 5.10 kg
ISO 306
 140 °C
@Load 1.02 kg
ISO 306
 
Processing PropertiesOriginal ValueComments
Feed Temperature 40.0 - 80.0 °C
Melt Temperature 220 - 260 °Cmass temperature
Mold Temperature 30.0 - 50.0 °C
Injection Velocity 100 - 200 mm/sec
Hold Pressure 30.0 - 60.0 MPa
 
Descriptive Properties
Back Pressurelow to medium
Screw Speedlow to medium

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Daplen™ ED117AE Polypropylene TPO Compound
Borealis Daplen™ EE108U Polypropylene TPO Compound
Borealis Daplen™ EE158AI Polypropylene TPO Compound
Borealis Daplen™ EE109AE TPO Compound
Borealis Daplen™ AK4504 TPO Compound

PBOREA404 / 108663

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.