MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Chesterton 622 White Grease
Categories: Fluid; Lubricant; Aluminum Gellant

Material Notes: Chesterton® 622 White Grease is a pure mineral oil grease with PTFE added designed for applications where a clean, nonstaining, food grade lubricant is required. It is a superior, multipurpose product that conforms with FDA regulation 178.3570 and 177.1550 for food machinery use. It is NSF registered as an H1 lubricant and can be used in federally inspected meat and poultry plants. It is a long lasting, non-hardening lubricant that withstand washout from water, steam, food or fruit juices. Chesterton 622 White Grease is virtually tasteless and odorless. When used on food processing equipment, users can be assured that the lubricant will not contaminate finished products.

Features:

  • NLGI #2
  • Excellent Water Resistance
  • PTFE Fortified
  • NSF H1 - Registration number 133929

Applications: A superior quality, clean, multi-purpose grease to lubricate slides, guides, moving parts of equipment in food, beverage, pharmaceutical, textile and other plants processing clean materials or packages. Use on bottle filling machinery, carton filling equipment, valves, pistons, pumps, paste and sauce fillers, conveyor belts and rollers, fruit feeders, meat packing equipment, canning machinery etc.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/cc
Viscosity Measurement 95Base Oil; ASTM D445
Kinematic Viscosity at 40°C (104°F) 12 cStBase Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 100 cStBase Oil; ASTM D445
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 41ASTM D2596
Four Ball Extreme Pressure, Weld Load 250 kgASTM D2596
Four Ball Wear 0.610 mmWeld Scar Diameter; ASTM D2266
Penetration 265 - 295ASTM D217
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 170 °C
Minimum Service Temperature, Air -23.0 °C
Dropping Point 245 °CASTM D2265
 
Descriptive Properties
AppearanceButtery, Translucent White
Consistency2NGLI
ThickenerAluminum Complex
Water Washout Resistance0.0245@80°C, ASTM D1264

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Water, H2O
Polyphosphazene Rubber (PZ, FZ)
Polynorbornene Rubber (PNR)
Polybutadiene Rubber (BR)
Parker Chomerics CHO-LUBE 4220 Electrically Conductive Grease

PPTCHS070 / 138182

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.