MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI LATAN 13 G/303 30% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, 30% Glass Fiber Reinforced

Material Notes: Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gears, cams, bushings, and other parts for the electromechanical, hydraulic, and automotive sectors, and others). A good resistance to hydrolysis makes it usable in hot water up to 80°-90°C. Basic Latan versions featuring low or high flowability are available, as well as an elastomer modified version to improve product toughness.

Specific Notes for this Material: 30% glass fiber; high rigidity.

Disclaimer from LATI: This document contains information based on average values as obtained from the results of laboratory tests and observations made on LATI materials. Tested materials were injection molded, used in their natural color, and conditioned in compliance with Standard ASTM D 618, procedure A. These values refer to LATI's best technical and scientific knowledge at the moment of testing and cannot be used as a basis for the development of applications. For a better assessment of the materials, you are kindly requested to contact LATI's technical or commercial offices, which are at your disposal and will supply detailed information on the most suitable characteristics for their intended use. With reference to DPR n.224 dated May 24, 1988, issued in accordance with EC Guide-lines 85/374, LATI Industria Termoplastici S.p.A. declines all responsibility arising from an improper use of the products described in this document.

All data provided by LATI.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccISO 1183
Water Absorption 0.20 %at 23°C; ISO 62
Linear Mold Shrinkage 0.0060 cm/cmLATI
Linear Mold Shrinkage, Transverse 0.0125 cm/cmLATI
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 85ASTM D785
Tensile Strength, Ultimate 83.0 MPaISO 527
 45.0 MPa
@Temperature 120 °C
ISO 527
 53.0 MPa
@Temperature 90.0 °C
ISO 527
 60.0 MPa
@Temperature 60.0 °C
ISO 527
Flexural Modulus 8.00 GPaASTM D790
 3.80 GPa
@Temperature 120 °C
ASTM D790
 4.50 GPa
@Temperature 90.0 °C
ASTM D790
 5.70 GPa
@Temperature 60.0 °C
ASTM D790
Izod Impact, Notched 0.550 J/cm
@Temperature -40.0 °C
ASTM D256
 55.0 J/m
@Temperature -20.0 °C
ASTM D256
 55.0 J/m
@Temperature 23.0 °C
ASTM D256
Charpy Impact Unnotched 1.80 J/cm²
@Temperature -20.0 °C
DIN 53453
 1.80 J/cm²
@Temperature -40.0 °C
DIN 53453
 2.00 J/cm²
@Temperature 23.0 °C
DIN 53453
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 23.0 kV/mm
@Thickness 2.00 mm
IEC 243-1
Comparative Tracking Index >= 600 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 165 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 162 °CASTM D648
Vicat Softening Point 156 °C50°C/h 50N; ISO 306
Flammability, UL94 HB
@Thickness 1.50 mm
Oxygen Index 18 %ISO 4589
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 210 °C
Mold Temperature 80.0 - 100 °C
Drying Temperature 80.0 - 100 °CNot essential, temperature can be reduced when using vacuum ovens.
Dry Time >= 3 hourNot essential, drying time can be reduced when using vacuum ovens.
 
Descriptive Properties
Heat Resistance - Ball Test (125°C)YIEC 335
Heat Resistance - Ball Test (165°C)NIEC 335
Injection Speedmedium
Needle Burner TestN1.47 mm
 N3.05 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hostaform® XGC25 POM, 25% Glass Reinforced
Delrin Delrin® 525GR NC000 POM-GF25
Delrin Delrin® 525GR BK000 POM-GF25
Celanese Hostaform® XGC25-LW01 POM, 25% Glass Reinforced
Celanese Hostaform® C 9021 GV1/30 GT POM, 26% Tribological

PLATI074 / 50072

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.