MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Parker Chomerics CHO-BOND® 592 Conductive Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: Highly conductive silver-filled epoxy adhesive which combines the best properties of metals and organics. This two-component system is unique in that it combines long pot life, good electrical conductivity, excellent adhesion, low temperature cure, easy mix ratio, low viscosity, low coefficient of thermal expansion, very low thermal impedance, and good thermal shock resistance.

Typical Applications: Connects dissimilar materials electrically and thermally; Excels as a sealant for microwave modules and components; Ideal for circuit board repair and grounding applications and Useful for EMI shielding

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.35 - 2.85 g/cc
Thickness 1.00 milRecommended
 
Mechanical PropertiesOriginal ValueComments
Shear Strength >= 1500 psiLap
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 0.050 ohm-cmDC
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 99.0 °C
Minimum Service Temperature, Air -62.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 80.0 °C
 5.00 min
@Temperature 302 °C
 15.0 min
@Temperature 125 °C
 30.0 min
@Temperature 100 °C
 168 hour
@Temperature 24.0 °C
produces lower electrical conductivity
Pot Life 240 - 360 min
@Temperature 25.0 °C
 2880 min
@Temperature 5.00 °C
Shelf Life 9.00 Month
 
Descriptive Properties
BinderEpoxy
ColorSilver
ConsistencyNearly Liquid
Coverage170.3 cm2/g
FillerAg
Mix Ratio100 to 50A:B
Working Life4 hrs

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHOME054 / 28276

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.