MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Honeywell TGP8000 Thermal Gap Pads
Categories: Other Engineering Material

Material Notes: Benefits And Features:
  • High thermal performance
  • Ultra-high compressibility for low stress applications
  • Excellent surface wetting for low contact resistance
  • High reliability
  • Electrically insulating
Overview: Honeywell Thermal Gap Pads (TGP) provide high thermal performance with ease of use across multitude of applications. Its ultra-high compressibility enables low stress and excellent conformity to mating surfaces. It is designed to minimize thermal resistance at interfaces, and maintain excellent performance through reliability testing. Honeywell TGP models are naturally tacky, and require no additional adhesive which could inhibit thermal performance. Products are available in thickness range from 0.5mm to 5.0mm.

Typical Applications:

  • Consumer electronics
  • Telecommunications & network servers
  • Automotive electronics
  • Power devices & modules
  • Semiconductors logics & memory

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.40 g/cc3.40 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore OO 3030ASTM D2240
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6.50e+15 ohm-cm6.50e+15 ohm-cmASTM D257
Dielectric Constant >= 8.3
@Frequency 1e+6 Hz
>= 8.3
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 8.00 W/m-K55.5 BTU-in/hr-ft²-°FASTM D5470
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorGrey
Thickness Range (mm)20.5-5ASTM D374

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHONWL6027 / 255357

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.