MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEM-PET80 Polyethylene Terephthalate (Bottles grade)
Categories: Polymer; Thermoplastic

Material Notes: Advantages:
  • With a good processability
  • Easy to shape
  • protect products, easy for transportation
  • Environmental Friendly
  • Impart the products to excellent characteristics
  • Strong compressive abilities
  • Organic Solvent resistance
  • Weather resistance
Applications:
  • Soda beverage bottle
  • Mineral water bottle
  • Cosmetic containers
  • Wide range of packaging materials
  • Aseptic ester for filling
  • A variety of fiber spinning
  • Alloy and composite materials
  • High-strength engineering plastic
  • Other special applications

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.830 - 0.930 g/cc
Density 1.20 - 1.60 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Value 25 - 45[meg/kg]
 
Thermal PropertiesOriginal ValueComments
Melting Point 245 - 255 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.40 %
 
Descriptive Properties
AppearanceCylinder Chip
Color<2.0B value
 >82L value
Composition<1.0 ppmAA content
 0.8-0.9 dl/gIV value
 1.1-1.5%DEG content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN794 / 267102

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.