MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nabaltec APYRAL® 200 SM Al(OH)3
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decomposition APYRAL ® does not generate toxic or corrosive gases. In addition, there is a distinct reduction in smoke density. APYRAL ® is effective in the crucial phase of the burning process before the outbreak of a fully developed fire.

APYRAL ® can be used as a flame retardant filler in

  • Thermosets
  • Elastomers
  • Thermoplastics
  • Cable Compounds
  • Technical Rubber Compounds
  • Pressed and cast Plastic Parts
  • Thermal Insulation Foams
  • Glass-fiber reinforced plastics

Information provided by Nabaltec.

Key Words: Aluminum Hydroxide, Al(OH)3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.200 g/cc0.00723 lb/in³
Density 2.40 g/cc0.0867 lb/in³
Brightness 98 %
@Wavelength 457 nm
98 %
@Wavelength 457 nm
Whiteness; Elrepho
Oil Absorption 48 %48 %(ml/100 g)
Moisture Absorption at Equilibrium 0.80 %0.80 %
Loss On Ignition 34.6 %34.6 %
Particle Size 0.40 µm0.40 µmMedian; Laser Diffraction
Specific Surface Area 15 m²/g15 m²/gBET
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 33
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 5000 ohm-cm5000 ohm-cm
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.581.58
 
Descriptive Properties
Aluminum Hydroxide (%)99.3
Sieve Analysis0.05%> 45 µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum Hydroxide, Gibbsite, Al(OH)3
Aluminum Hydroxide, Bayerite, Al(OH)3
Alpha Calcit Alfrimal 446 Aluminum Hydroxide 99.5%
Nabaltec NH 20 Aluminum Hydroxide
Nabaltec APYRAL® 1E Al(OH)3

CNABAL16A / 159800

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.