Standard Applications: RHODOLINE© 225 is a low foaming anionic dispersant designed for exterior coatings. It is effective in formulations containing reactive pigments. Use RHODOLINE© 225 at 5 to 15 pounds per gallon of finished paint. The optimum use level of RHODOLINE© 225 may be determined by the pigment dispersant demand method. Chemical Name: ACRYLIC POLYMER SOLUTION CAS No: 7732-18-5, 54193-36-1 Information provided by Solvay |