MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECANYL™ MT XRO Autoclavable Polymer
Categories: Polymer; Thermoplastic

Material Notes: TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease and tool friendliness of acetal or POM. This allows part designers to take advantage of lower manufacturing costs by increasing output rates, and reducing tool wear, all without sacrificing part performance. TECANYL™ MT and TECANYL™ MT XRO shapes are all ISO 10993 tested to support their use in instrumentation that is intended to come in contact with blood and tissue for a period of not more than 24 hours. Ensinger can also provide TECANYL™ MT grades in finished injection molded parts for high volume applications.

  • Excellent autoclave performance comparable to higher temperature materials
  • Easily machined, producing high quality surface
  • No black speck generation as in sulfone polymers
  • Lower manufacturing costs
  • ISO 10993 Tested

Information Provided by Ensinger Industries, Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/ccASTM D792
Density 0.0300 lb/in³ISO 1183
Water Absorption 0.23 %
@Temperature 22.8 °C
equilibrium; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 9800 psi
@Temperature 22.8 °C
ASTM D638
Elongation at Break 16.3 %
@Temperature 22.8 °C
ASTM D638
Tensile Modulus 471000 psi
@Temperature 22.8 °C
ASTM D638
Flexural Strength 14600 psi
@Temperature 22.8 °C
ASTM D790
Flexural Modulus 368000 psi
@Temperature 22.8 °C
ASTM D790
Izod Impact, Notched 2.60 ft-lb/in
@Temperature 22.8 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 48.1 µin/in-°F
@Temperature -40.0 - 37.8 °C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 296 °FASTM D648
Vicat Softening Point 168 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyphenylsulfone (PPSU)
Evonik Europlex® PPSU Polyphenylsulfone Engineering Plastic
Evonik Europlex® PPSU High Performance Sheet
Evonik EUROPLEX® PPSU 99470/99472 Transparent sheet
Evonik EUROPLEX® PPSU 99460 H Opaque Sheet

PENSIN009 / 92826

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.