MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polymax® Maxelast® P2620 TPE, PP Overmold or Standalone use
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polypropylene (PP)

Material Notes: Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.
    Uses:
  • Consumer Products
  • Toys & Novelties
  • Auto Parts
  • Tool Hand Grips
  • Sporting Goods
  • Wire & Cable Electronics
  • Medical Devices
  • Plastic Toughening

Information from Alliance Polymers & Services, Distributor of Nantong Elastomer Technology Co.Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 22
@Time 10.0 sec
ASTM D2240
Tensile Strength, Yield 167 psiASTM D412
Elongation at Break 880 %ASTM D412
100% Modulus 0.0827 ksi
@Strain 100 %
ASTM D412
300% Modulus 0.131 ksi
@Strain 300 %
ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polymax® Maxelast® A9810 TPE, ABS/PC Overmold
Avient Gravi-Tech™ GRV-TP-080-W-NAT Styrene Butadiene Block Copolymer (SBC)
Avient Elastamax™ XL 0234-1 SEBS-Based Thermoplastic Elastomer
AlphaGary Evoprene™ G 3290 SEBS Thermoplastic Elastomer
AdvanSource Biomaterials ChronoPrene™ 25A Thermoplastic Rubber Elastomer

PMAXEL130 / 121217

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.