MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Flexible A85UB Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes:

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 7915 sec; ASTM D2240
 85ASTM D2240
Tensile Strength at Break 16.5 MPa510 mm/min; ASTM D638
Tensile Stress at Strain 8.27 MPa
@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 420 %510 mm/min; ASTM D638
Tear Strength 73.6 kN/mDie C, 510 mm/min; ASTM D624
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -32.8 °CASTM D746
Flammability, UL94 HBUL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 174 - 179 °C
 193 - 204 °C
 
Descriptive Properties
AdditiveBiocide
 UV Stabilizer
AppearanceClear/Transparent
FeaturesUV Absorbing
FormsPellets
Generic MaterialPVC, Flexible
Generic NamePolyvinyl Chloride, Flexible
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesFlooring
 Hose
 Tubing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Wire & Cable W3400L Polyvinyl Chloride, Flexible
Geon® Performance Solutions Vinyl Wire & Cable MAF110A Polyvinyl Chloride, Flexible

PH0POL0409 / 144978

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.