MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayhydur® BL 5335 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydur BL 5335 is a hydrophilized, blocked aliphatic polyisocyanate based on Desmodur® W. It is suitable in combination with Bayhydrol® grade OH-functional polymers for the formulation of lightfast, single-component polyurethane baking coatings.

Properties / Applications: Bayhydur BL 5335 is a blocked polyisocyanate and was developed for industrial use. It is used as a hardener for the formulation of lightfast one-component polyurethane baking coatings suitable for spray, dip or roller application. The product is preferably used in glass coating applications. As with any product, use of Bayhydur BL 5335 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/cc
Volatiles 64 - 66 %64 - 66 %1 g / 1 h / 105°C
pH 10 - 3010 - 30
 
Thermal PropertiesMetricEnglishComments
Flash Point 59.0 °C138 °F
 
Descriptive Properties
Content7.1%NCO content, blocked (solid resin)
Flow time10-30s4 mm cup

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Applied Nanotech Ag-iJ10 Silver Ink
Versalis Intex® 2740 Styrene - Butadiene Copolymer
Momentive Performance Materials HPC Boron Nitride (BN)/TiO2 Water Based Coating
Kazanorgsintez Demulsifying Reagent of Reapon-4B Grade
Covestro Bayhydur® BL XP 2706 Polyurethane Coating

PCOVEST0196 / 201979

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.