MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Lord Adhesives Thermoset™ MT-322 Thermally Conductive Adhesive
Categories: Polymer; Adhesive

Material Notes: LORD Thermoset™ MT-322 thermally conductive adhesive is a one-component silicone adhesive designed for use in assemblies where thermal dissipation is desired. Thermoset MT-322 adhesive can be used to bond electronic devices such as memory chips to lids, heat spreaders and heat sinks. The adhesive cures to form a flexible elastomer offering superior high temperature electrical properties.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.65 g/cc2.65 g/cc
Viscosity 65000 cP
@Temperature 25.0 °C
65000 cP
@Temperature 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM D2240
Shear Strength 2.10 MPa
@Temperature 304.5 °C
305 psi
@Temperature 580.1 °F
ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm
@Temperature 25.0 °C
2.00e+15 ohm-cm
@Temperature 77.0 °F
ASTM D257
Dielectric Constant 2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 160 µm/m-°C88.9 µin/in-°F
Thermal Conductivity 1.70 W/m-K11.8 BTU-in/hr-ft²-°FMathis Hot Disk Analyzer
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 150 °C
0.500 hour
@Temperature 302 °F
 60.0 min
@Temperature 120 °C
1.00 hour
@Temperature 248 °F
Pot Life 43200 min
@Temperature 25.0 °C
43200 min
@Temperature 77.0 °F
Shelf Life 12.0 Month
@Temperature -40.0 °C
12.0 Month
@Temperature -40.0 °F
 
Descriptive Properties
AppearanceGray
ConsistencyPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD037 / 86045

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.