MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Honeywell HT5000 Thermally Conductive Gap Fillers
Categories: Polymer; Thermoset; Silicone

Material Notes: Benefits And Features:
  • High thermal performance
  • low contact resistance
  • Easily dispensable and reworkable
  • High compressibility for low stress applications
  • Reliable thermal performance
  • No pump out and cracking risk
Overview: Honeywell HT one-part series Gap Filler provides an effective thermal properties and high conformability with its high compressibility. It is formulated to deliver high dispense rates for improved productivity, long-term reliability performance and easy reworkability. It is designed to minimize thermal resistance at interfaces, maintain excellent performance through reliability testing, and provide scalable application at a competitive cost.

Typical Applications:

  • Consumer electronics
  • Telecommunications equipment
  • Automotive electronics
  • Power supplies & semiconductors
  • Memory & power modules
  • Power electronics

Information provided by Honeywell

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 3.40 g/cc3.40 g/ccASTM D792
Outgassing - Total Mass Loss <= 0.50 %<= 0.50 %ASTM E595
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 5.00 W/m-K34.7 BTU-in/hr-ft²-°FASTM D5470
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
ColorGrey
Dispense Rate>10 g/min90 Psi, 30cc EFD syringe
Minimum BLT0.05 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHONWL6003 / 255333

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.