SBR 1502 is a light-colored, general purpose cold SBR elastomer It provides the maximum in physical properties along with excellent color characteristics. Unique Features: - Cold polymerized styrene-butadiene elastomer
- Lighter color and FDA 21 CFR §177.2600 compliant
Applications:- Calendared soles
- Household products such as floor tiles
- Mechanical rubber goods
Information provided by Lion Elastomer |